Physical Properties Metric English Comments
Bulk Density 0.0150 g/cc
0.000542 lb/in³
Minimum
SYNTHOS Koplen® 1020 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to blocks.Specific Characteristics: Flammability according to..
Bulk Density 0.0150 - 0.0400 g/cc
0.000542 - 0.00145 lb/in³
Typical
SYNTHOS Koplen® 1020 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: By water steam or hot water, the volume of the beads is increased. Foam-processing to blocks.Specific Characteristics: Flammability according to..
Bulk Density 0.0150 g/cc
0.000542 lb/in³
Minimum
SYNTHOS Koplen® 1640 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO ..
Bulk Density 0.0150 - 0.0300 g/cc
0.000542 - 0.00108 lb/in³
Typical
SYNTHOS Koplen® 1640 F Expandable Polystyrene
Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks.Specific Characteristics: Flammability according to CSN EN ISO ..
Bulk Density >= 0.0150 g/cc
>= 0.000542 lb/in³
Typical
SYNTHOS Koplen® 2040 FR Expandable Polystyrene
Low Pentane Self-Extinguishing type Koplen®.Processing Method: Pre-expansion of beads by water steam, hot water or hot air. Shaping into blocks. Lower density can be achieved after several prefor..
Bulk Density 0.0150 - 0.0190 g/cc
0.000542 - 0.000686 lb/in³
BASF Neopolen® P 8220 K 0.02 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Bulk Density 0.0150 - 0.0190 g/cc
0.000542 - 0.000686 lb/in³
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Bulk Density 0.0150 - 0.0190 g/cc
0.000542 - 0.000686 lb/in³
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..