| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measure | 200 cSt | 200 cSt | |
| Dow Corning 670 Fluid A blend of approximately 50 percent cyclopentasiloxane and approximately 50 percent polypropylsilsesquioxane, especially useful in color cosmetic formulations.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 - 500 cSt | 200 - 500 cSt | Kinetic/Kinematic |
| Dow Corning Q4-3667 Fluid Silicone polyether (glycol) copolymer.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 cSt | 200 cSt | Kinetic/Kinematic |
| Dow Corning SYL-OFF® PMCP7040 Coating Syl-Off® 7040 Coating is a 100% active solids coating containing a low viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for fast cure and stable release against agg.. |
|||
| Viscosity Measure | 200 cSt | 200 cSt | Kinetic/Kinematic |
| Dow Corning SYL-OFF® PMCPSL 9111 Coating Syl-Off® SL 9111 Coating is a solvent-free, low temperature cure release coating for filmic pressure sensitive laminate/labelstock.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 cSt | 200 cSt | Kinetic/Kinematic |
| Dow Corning XIAMETER® PMCPPMX-200 200CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 200CS. 100% active, 200 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 cSt | 200 cSt | Kinetic/Kinematic |
| Dow Corning 2-2617 Diesel Antifoam 100% active polysilicone polyether copolymer, used to control foam in diesel fuel.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 - 500 cSt | 200 - 500 cSt | Kinetic/Kinematic |
| Dow Corning XIAMETER® XIAMETER ® MEM-1665 Emulsion Is chemically equivalent to DOW CORNING® 1665 EMULSION. A 55% active, silicone emulsion of medium viscosity polydimethylsiloxane fluid.Information provided by Dow Corning |
|||
| Viscosity Measure | 200 cSt @Temperature 55.0 °C |
200 cSt @Temperature 131 °F |
|
| Dow TONE™ 305 Polyol TONE™ 0305 polyol is a very low equivalent weight tri-functional liquid polyol for use in urethane cast elastomers, coatings, adhesives and soft foams.Information provided by Dow |
|||
| Viscosity Measure | 200 cSt | 200 cSt | Kinetic/Kinematic |
| Dow Corning XIAMETER® PMCPMEM-1664 Fluid Is chemically equivalent to DOW CORNING® 1664 EMULSION. Non-ionic, 50% active emulsion based on high viscosity polydimethylsiloxane.Information provided by Dow Corning |
|||