Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 350000 - 575000 cSt | 350000 - 575000 cSt | Kinetic/Kinematic |
Dow Corning EL-8050 ID Silicone Organic Elastomer Blend Combine the feel of silicone elastomer gels with a wider range of organic ingredients and actives. Our silicone organic elastomer blends can give you the innovative freedom to create color cosmetics.. |
|||
Viscosity Measure | 350000 - 575000 cSt | 350000 - 575000 cSt | Kinetic/Kinematic |
Dow Corning EL-9140 DM Silicone Elastomer Blend This product can be used in a wide range of personal care products as a rheology and texture modifier in oil-in-water and water-in-oil emulsions and anhydrous gels.Dow Corning® EL-9140 DM Silicone .. |
|||
Viscosity Measure | 350000 - 490000 cSt | 350000 - 490000 cSt | Kinetic/Kinematic |
Dow Corning ST Elastomer 10 A blend of a unique silicone elastomer and a volatile silicone fluid for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning |
|||
Viscosity Measure | 350000 - 575000 cSt | 350000 - 575000 cSt | Kinetic/Kinematic |
Dow Corning EL-8051 IN Silicone Organic Elastomer Blend Combine the feel of silicone elastomer gels with a wider range of organic ingredients and actives. Our silicone organic elastomer blends can give you the innovative freedom to create color cosmetics.. |