Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1500 cSt | 1500 cSt | kinetic/kinematic |
Dow Corning 1503 Fluid A blend of an ultra high viscosity dimethiconol in a low viscosity dimethicone fluid for use in skincare, woundcare, scar therapy, suncare, and color cosmetic applications.Information provided by Do.. |