Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 10000 cSt | 10000 cSt | Kinetic/Kinematic |
Dow Corning BY 25-320 This is a clear viscous liquid, where approximately 20% of an ultra high viscosity Dimethicone gum is dispersed into iso-paraffin.Areas of potential use for BY 25-320 encompass a wide range of Cosme.. |
|||
Viscosity Measure | 10000 cSt | 10000 cSt | Kinetic/Kinematic |
Dow Corning FS 1265 Fluid, 10,000 CST 100% active, fluorosilicone polymer.Information provided by Dow Corning |
|||
Viscosity Measure | 10000 cSt | 10000 cSt | |
Dow Corning XIAMETER® PMCPPMX-200 10,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10,000CS. 100% active, 10,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Viscosity Measure | 10000 cSt | 10000 cSt | Kinetic/Kinematic |
Dow Corning 2-1865 Microemulsion Translucent, 40% active, pourable anionic / non-ionic microemulsion with a polydimethylsiloxane / cyclic blend internal phase.Information provided by Dow Corning |