Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning ES-5612 Silicone Formulation Aid Produces W/Si and W/Si+O emulsions with textures that range from lotion to cream, leaving a light, nongreasy after feel on the skin.It is a low molecular weight ethoxylated silicone surfactant.Dow C.. |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning FS 1265 Fluid, 1000 CST 100% active, fluorosilicone polymer.Information provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning Q2-5220 Resin Modifier A silicone glycol copolymerInformation provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning Q7-9120 Silicone Fluid, 1000 CST Polydimethylsiloxane fluid, excipient for pharmaceutical and cosmetic applications.Information provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | kinetic/kinematic |
Dow Corning 200® 1000 CST FLUID 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | |
Dow Corning XIAMETER® PMCPPMX-200 1000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 1,000CS. 100% active, 1000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning 360 Medical Fluid, 1000 CST. Colorless and odorless polydimethysiloxane fluid for lubrication and siliconization of glass, metals, plastics and rubber in medical applications.Information provided by Dow Corning |
|||
Viscosity Measure | 1000 cSt | 1000 cSt | Kinetic/Kinematic |
Dow Corning 5200 Formulation Aid An alkylmethyl siloxane copolyol designed to prepare stable water-in-oil emulsions.Information provided by Dow Corning |