Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0032 - 0.0041 cm/cm @Time 86400 sec |
0.0032 - 0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0032 - 0.0041 cm/cm @Time 86400 sec |
0.0032 - 0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding. Mold Release, Statically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0032 - 0.0041 cm/cm @Time 86400 sec |
0.0032 - 0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC (Asia Pacific) LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0032 - 0.0041 cm/cm @Time 86400 sec |
0.0032 - 0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0032 - 0.0041 cm/cm @Time 86400 sec |
0.0032 - 0.0041 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |