Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0214 - 0.023 cm/cm @Time 86400 sec |
0.0214 - 0.023 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0214 cm/cm @Time 86400 sec |
0.0214 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0214 cm/cm @Time 86400 sec |
0.0214 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0214 cm/cm @Time 86400 sec |
0.0214 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |