Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer
LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004AH Acetal Homopolymer
LNP* LUBRICOMP* KP004AH is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer
LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp KP004AXZ Acetal Homopoly
LNP* Lubricomp* KP004AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP..
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER
LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 - 0.029 cm/cm

@Time 86400 sec
0.021 - 0.029 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer
LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 - 0.023 cm/cm

@Time 86400 sec
0.021 - 0.023 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am..
Linear Mold Shrinkage, Transverse 0.021 - 0.023 cm/cm

@Time 86400 sec
0.021 - 0.023 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As..
Linear Mold Shrinkage, Transverse 0.021 - 0.024 cm/cm

@Time 86400 sec
0.021 - 0.024 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT
LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer
LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release.
Linear Mold Shrinkage, Transverse 0.021 cm/cm

@Thickness 3.00 mm
0.021 in/in

@Thickness 0.118 in
ISO 294-4
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)