Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0052 cm/cm @Time 86400 sec |
0.0045 - 0.0052 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0052 cm/cm @Time 86400 sec |
0.0045 - 0.0052 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0052 cm/cm @Time 86400 sec |
0.0045 - 0.0052 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific) LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 cm/cm @Time 86400 sec |
0.0045 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0052 cm/cm @Time 86400 sec |
0.0045 - 0.0052 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |