Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Linear Mold Shrinkage, Transverse | 0.022 cm/cm @Time 86400 sec |
0.022 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |