Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP KF002 Acetal Copolymer LNP THERMOCOMP* KF002 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66 LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOTUF WF006I PBT LNP THERMOTUF* WF006I is a compound based on PBT containing 30% Glass Fiber. Added features of this material include: High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP KF002XXP Acetal Copoly LNP* Thermocomp* KF002XXP is a compound based on Acetal Copolymer resin containing 10% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0129 cm/cm @Time 86400 sec |
0.0129 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg.. |