Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0078 cm/cm @Time 86400 sec |
0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant. |
|||
Linear Mold Shrinkage, Transverse | 0.0078 cm/cm @Time 86400 sec |
0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA 6/10 (Asia Pacific) LNP* Lubricomp* QCL349 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, Flame Retardant, Elect.. |
|||
Linear Mold Shrinkage, Transverse | 0.0078 cm/cm @Time 86400 sec |
0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0078 cm/cm @Time 86400 sec |
0.0078 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |