Polymer Property : Linear Mold Shrinkage, Transverse = 0.0045 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0045 - 0.0052 cm/cm

@Time 86400 sec
0.0045 - 0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..
Linear Mold Shrinkage, Transverse 0.0045 - 0.0052 cm/cm

@Time 86400 sec
0.0045 - 0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive. Wear Resistant, Flame Retardant.
Linear Mold Shrinkage, Transverse 0.0045 - 0.0052 cm/cm

@Time 86400 sec
0.0045 - 0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific)
LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS
LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic.
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS (Asia Pacific)
LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat.
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC
LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific)
LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.0045 - 0.0052 cm/cm

@Time 86400 sec
0.0045 - 0.0052 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific)
LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup..