Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific) LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural. |