Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco HiPerSYN™ ISO 32 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco HiPerSYN™ ISO 46 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco HiPerSYN™ ISO 68 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Clarity® 10W-20 Synthetic Hydraulic Oil AW Chevron Clarity Synthetic Hydraulic Oil AW is designed to give maximum protection to both mobile and stationary hydraulic pumps in high-performance industrial applications as well as in environmenta.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Clarity® ISO 32 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Clarity® ISO 46 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |
|||
Oxidative Stability | >= 18000 hour | >= 18000 hour | Hours to 2.0 mg KOH/g acid number; ASTM D943 |
ChevronTexaco Clarity® ISO 68 Hydraulic Oil AW FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are.. |