Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | >= 100 g/m² | >= 62.5 lb/ream | double-sided |
ArcelorMittal Extragal® Z100 Double-sided pure zinc galvanized steel Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib.. |
|||
Coating Weight | 100 - 120 g/m² | 62.5 - 75.0 lb/ream | per side |
ArcelorMittal Extragal® Z200 Double-sided pure zinc galvanized steel Applications: Because of their high corrosion protection capacity and surface quality, Extragal® coated products are recommended for numerous automotive applications, for both visible and non-visib.. |
|||
Coating Weight | >= 100 g/m² | >= 62.5 lb/ream | double-sided |
ArcelorMittal Ultragal® Z100 Zinc coatings and thin organic coating Applications: With its ability to limit repeated waviness during deformation, combined with the proven qualities of Extragal(surface quality, corrosion protection), Ultragal is a coating specificall.. |
|||
Coating Weight | >= 100 g/m² | >= 62.5 lb/ream | |
ArcelorMittal AS100 Aluminized steel Applications: Alusi® coating is resistant to heat, high temperature oxidation and corrosion, and offers a high level of reflectivity, making it suitable for applications in a corrosive atmosphere .. |