Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Coating Weight 490 g/m²
306 lb/ream
entire thickness; NF EN ISO 2286.2
Isoflon Tisoflon® 10K Polytetrafluoroethylene Coated Kevlar Fabric
PTFE coated Kevlar fabric TISOFLON®Information provided by Isoflon.
Coating Weight 490 g/m²
306 lb/ream
entire thickness; NF EN ISO 2286.2
Isoflon Tisoflon® 14S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.