Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 31.4 g/m² | 19.6 lb/ream | 520 |
ExxonMobil Bicor® 140 BSR-ONE OPP Film Product Description: Bicor BSR-ONE is a two-side sealable, one side treated, coextruded OPP film designed for unsupported plain or surface print applications, and in laminations on both HFFS and VF.. |
|||
Coating Weight | 31.4 g/m² | 19.6 lb/ream | ExxonMobil Method |
ExxonMobil Label-Lyte™ 35LL400 OPP Film Product Description: A one-side treated, transparent coextruded OPP film. The film is slip controlled for optimal performance on reel-fed labeling machines.Availability: Africa & Middle East, Asia .. |
|||
Coating Weight | 31.4 g/m² | 19.6 lb/ream | ExxonMobil Method |
ExxonMobil Oppalyte™ 40MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |