Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 27.0 g/m² | 16.9 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 120 AB-X OPP Film Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as.. |
|||
Coating Weight | 27.0 g/m² | 16.9 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 120 XRG-2 OPP Film Product Description: Bicor 120 XRG-2 is a one-side sealable OPP film that can be used as the inside web of a lamination where exceptional seal performance is required. The high-energy surface is int.. |
|||
Coating Weight | 27.0 g/m² | 16.9 lb/ream | ExxonMobil Method |
ExxonMobil Bicor® 120 LTSC OPP Film Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS.. |