Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 24.8 g/m² | 15.5 lb/ream | ExxonMobil Method |
ExxonMobil Metallyte™ UHB 35 MWHB OPP Film Product Description: A multi-layer, cavitaed, white OPP film structure that has exceptional barrier to gases and flavors. It is metalized on one side and treated on the other. It is designed for use.. |
|||
Coating Weight | 24.8 g/m² | 15.5 lb/ream | ExxonMobil Method |
ExxonMobil Metallyte™ UHB 35MU842 OPP Film Product Description: A metalized high opacity white oriented polypropylene film. It is biaxially oriented, multi-layer polypropylene film with aluminum deposited on an adhesion promoting layer. The .. |
|||
Coating Weight | 24.8 g/m² | 15.5 lb/ream | ExxonMobil Method |
ExxonMobil OPPalyte® 278 WOS-2 OPP Film Product Description: One-side treated, on-side sealable, white opaque OPP film with a proprietary cavitated core. WOS-2 was developed to provide improvements over 278 WOS in terms of lower and more .. |