Physical Properties | Metric | English | Comments |
---|---|---|---|
Coating Weight | 17.8 g/m² | 11.1 lb/ream | ExxonMobil Method |
ExxonMobil Bicor™ 20MB668 OPP Film Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid.. |