Physical Properties | Metric | English | Comments |
---|---|---|---|
Neck In | 3.56 cm | 1.40 in | 164 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Neck In | 3.56 cm | 1.40 in | 328 ft/min, Constant output at 35 rpm; ExxonMobil Method |
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |