Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 51.58 cSt @Temperature 21.0 °C |
51.58 cSt @Temperature 69.8 °F |
ASTM D 445 |
ConocoPhillips Hydroclear® 22 Ultra-Clean Spindle Oil Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o.. |