Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 200 cSt | 200 cSt | |
Dow Corning MOLYKOTE® PG-21 PLASTISLIP GREASE Silicone grease especially for plastic/plastic and plastic/metal combinations like control cables and circuit lever systemInformation provided by Dow Corning |
|||
Kinematic Viscosity | 200 cSt | 200 cSt | |
Dow Corning MOLYKOTE® PG-54 PLASTISLIP GREASE Silicone grease with solid lubricantsInformation provided by Dow Corning |
|||
Kinematic Viscosity | 200 cSt @Temperature 25.0 °C |
200 cSt @Temperature 77.0 °F |
|
Dow Corning SYL-OFF® 7040 COATING Syl-Off® 7040 Coating is a 100% active solids coating containing a low viscosity hexenyl endblocked and pendant functional silicone polymer. Recommended for fast cure and stable release against agg.. |
|||
Kinematic Viscosity | 200 cSt | 200 cSt | |
Dow Corning SYL-OFF® SL 9111 COATING Syl-Off® SL 9111 Coating is a solvent-free, low temperature cure release coating for filmic pressure sensitive laminate/labelstock.Information provided by Dow Corning |
|||
Kinematic Viscosity | 200 cSt | 200 cSt | |
Dow Corning 1664 EMULSION Non-ionic, 50% active emulsion based on high viscosity polydimethylsiloxane.Information provided by Dow Corning |
|||
Kinematic Viscosity | 200 - 500 cSt | 200 - 500 cSt | |
Dow Corning 1665 EMULSION Dow Corning® 1665 Emulsion is a milky white cationic emulsion of an intermediate viscosity polydimethylsiloxane fluid. The emulsion contains 55% silicone and has a relatively low particle size.Info.. |
|||
Kinematic Viscosity | 200 cSt | 200 cSt | |
Dow Corning 1785 EMULSION A 60 percent anionic emulsion of high molecular weight polydimethylsiloxane for use in shower gels and hair care applications.Information provided by Dow Corning |