Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity | 1500 cSt @Temperature 20.0 °C |
1500 cSt @Temperature 68.0 °F |
ASTM D445 |
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Kinematic Viscosity | 1500 cSt | 1500 cSt | |
Dow Corning HV 600 EMULSION Non-ionic, 50% active emulsion based on high viscosity polydimethylsiloxane.Information provided by Dow Corning |
|||
Kinematic Viscosity | 1500 cSt | 1500 cSt | |
Dow Corning MOLYKOTE® 1122 CHAIN AND OPEN GEAR GREASE Lubricating chains, gear drives, worm gears, slow-moving bearings. Resists water, steam and high temperatures; contains MoS2 for high loads and low speeds. Thick, black, tacky synthetic grease con.. |