Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR .. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B100MP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B100QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B100ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B135MP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B135QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B135ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B73QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B85QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | ASTM Test |
BASF Capron® B85ZP Nylon 6 (DAM) (America)
(discontinued **) Not Impact modified.Information provided by BASF.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m²/day, No thickness given |
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a.. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | Average value: 14.0 cc-mm/m²-24hr-atm Grade Count:17 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B73MP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | cc/m2/day (Thickness not reported) |
BASF Capron® B73ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Nitrogen Transmission | 14.0 cc-mm/m²-24hr-atm | 35.6 cc-mil/100 in²-24hr-atm | Average value: 14.0 cc-mm/m²-24hr-atm Grade Count:10 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |