Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | Average value: 104 cc-mm/m²-24hr-atm Grade Count:25 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EP-521 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1500 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proc.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1539 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Multiple coats, up to 2,000 microns.Processing Method.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1810 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-1 FEP Dispersion, Translucent White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-2 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-4 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-4GY FEP Dispersion, Gray NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0012 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0025 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0050 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0100 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0250 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0500 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-1000 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-1500 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-2400 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1830 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Nitrogen Transmission | 104 cc-mm/m²-24hr-atm | 263 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON EP-541 ETFE Pellets Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl.. |