Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 3500 - 7500 cc-mm/m²-24hr-atm | 8890 - 19100 cc-mil/100 in²-24hr-atm | Average value: 4500 cc-mm/m²-24hr-atm Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |