Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 1.646 cc-mm/m²-24hr-atm @Thickness 0.0250 mm |
4.181 cc-mil/100 in²-24hr-atm @Thickness 0.000984 in |
DIN 53380-2 |
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |