| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 5.80 - 6.00 g/cc | 0.210 - 0.217 lb/in³ | |
|
Pacific Sintered Materials FC-203-N Copper Iron Powdered Metal
Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-1000-20All information provided by Pacific Sintered Metals.
|
|||
| Density | 5.80 - 6.00 g/cc | 0.210 - 0.217 lb/in³ | |
|
Pacific Sintered Materials FC-208-N Copper Iron Powdered Metal
Applications:Excellent for self-lubricating parts and heavy duty bearingsEquivalent MPIF Specification: FC-2000-K40All information provided by Pacific Sintered Metals.
|
|||
| Density | 5.80 - 6.00 g/cc | 0.210 - 0.217 lb/in³ | |
|
PSM Industries Pacific Sintered Metals Copper Iron FC-203-N Powdered Metal
Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-1000-20Information Provided by Pacific Sintered Metals, a division of PSM Industries
|
|||
| Density | 5.80 - 6.00 g/cc | 0.210 - 0.217 lb/in³ | |
|
PSM Industries Pacific Sintered Metals Copper Iron FC-208-N Powdered Metal
Excellent for self-lubricating parts and heavy duty bearings. Equivalent MPIF Specification: FC-2000-K40Information Provided by Pacific Sintered Metals, a division of PSM Industries
|
|||
| Density | 5.80 g/cc | 0.210 lb/in³ | |
|
Pyrotek MC-1 Metal Ceramic Thermocouple Protection Tube
For casting, MC-1 thermocouple protection tubes are a unique blend of metal and ceramic, exhibiting properties not found solely in either individual material. MC-1 tubes offer high thermal conducti..
|
|||
| Density | 5.80 g/cc | 0.210 lb/in³ | |
|
MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
|
|||
| Density | 5.80 g/cc | 0.210 lb/in³ | apparent |
|
Wall Colmonoy COLMONOY® 80 PTA - Nickel-Base Hard Surfacing Composite Powder
Description: Colmonoy 80 PTA is a unique composite material containing a high volume percent of extremely abrasion resistant tungsten carbide particles (3500 DPH) in a soft (HRC 30) impact resistant..
|
|||
| Density | 5.80 - 6.30 g/cc | 0.210 - 0.228 lb/in³ | |
|
China Tungsten ST1460 PM Antifriction Parts
Information provided by China Tungsten
|
|||
| Density | 5.80 g/cc | 0.210 lb/in³ | |
|
3M Micro Milling Media ZGC
High performance meets low price High densityHigh wear resistanceHigh milling efficiencyExtremely fine microstructureInformation provided by 3M
|
|||