Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.909 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 0.909 g/cc
0.0328 lb/in³
ASTM D4883
Eastman 812A Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D4883
Eastman 812P Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet...
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene
09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe
Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethy..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D1505
Westlake EM812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D792
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..
Density 0.909 g/cc
0.0329 lb/in³
ConocoPhillips Conoflex® 32 SRI Lubricant ISO
Description: Conoco Conoflex SRI Lubricant is an excellent wire rope lubricant and preservative for any metal product, particularly when protecting from saltwater. It lubricates and preserves the wi..
Density 0.909 g/cc
0.0328 lb/in³
ASTM D792
Ineos H07G-00 Polypropylene Homopolymer
Grade H07G-00 is a barefoot polypropylene homopolymer designed for cast film applications and flexible packaging. This grade has good optical properties and consistent processing. This grade meets t..