| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | Polymerized; ASTM D792 |
| Proto3000 Objet TangoBlack FullCure970 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | Polymerized; ASTM D792 |
| Proto3000 Objet TangoBlackPlus FullCure980 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | Polymerized; ASTM D792 |
| Proto3000 Objet TangoPlus FullCure930 Rubber-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
| Density | 1.08 - 1.13 g/cc | 0.0390 - 0.0408 lb/in³ | Average value: 1.11 g/cc Grade Count:5 |
| Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
| Density | 1.01 - 1.13 g/cc | 0.0365 - 0.0408 lb/in³ | Average value: 1.11 g/cc Grade Count:6 |
| Overview of materials for Solventless Epoxy Varnish, Electrical Insulation This property data is a summary of similar materials in the MatWeb database for the category "Solventless Epoxy Varnish, Electrical Insulation". Each property range of values reported is minimum and.. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | |
| Fibre Glast 2000 / 2020 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | |
| Fibre Glast 2000 / 2120 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
| Density | 1.08 - 1.13 g/cc | 0.0390 - 0.0408 lb/in³ | OSTM059 |
| Solvay TOLCIDE® PS 20A 20% tetrakis hydroxymethyl phosphonium sulfate Identification: Proprietary formulation based upon TETRAKIS (HYDROXYMETHYL) PHOSPHONIUM SULPHATE (THPS CAS NR 55566-30-8) and a biopenetrantAvailable in: North AmericaFoam potential: Non-foamingFunc.. |
|||
| Density | 1.02 - 1.13 g/cc | 0.0368 - 0.0408 lb/in³ | Free flowing, Typical |
| Solvay Chemicals Soda Solvay® Dense Soda Ash (European Grade) Soda Ash Dense is the grade preferred for glass manufacture because its granular properties make it dust-free and reduce the risks of segregation during transport and handling.Applications: Glass in.. |
|||
| Density | 1.07 - 1.13 g/cc | 0.0387 - 0.0408 lb/in³ | |
| Shandong Guangyin PA 610 Nylon Resin Features and Applications: Compared with nylon 6 and nylon 66, nylon 610 is much softer and lower in water absorption, featured by excellent low temperature resistance and dimensional stability. Due.. |
|||
| Density | 1.11 - 1.13 g/cc | 0.0401 - 0.0408 lb/in³ | OSTM058 |
| Solvay ALBRITECT® PM1 Triethylphosphonoacetate Identification: TriethylphosphonoacetateCAS: 867 – 13 – 0Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALBRITECT PM1 is an excellent thermal and color s.. |
|||
| Density | 1.10 - 1.13 g/cc | 0.0397 - 0.0408 lb/in³ | ASTM D792 |
| Cast Nylons Nycast® CP Caprolactam/Laurinlactum Copolymer Cast Nylon Highly resilient, with higher tensile elongation and impact strength than standard grades, NYCAST® CP is used applications requiring an extra degree of toughness. A copolymer of caprolactam and lau.. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | |
| BASF Triethanolamine Pure Formula: C6H15NO3CAS: 102-71-6Description: Triethanolamine Pure is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions.Synonyms: Triethanolamine, 2,2'.. |
|||
| Density | 1.12 - 1.13 g/cc | 0.0405 - 0.0408 lb/in³ | |
| BASF Triethanolamine Pure Formula: C6H15NCAS: 102-71-6Description Triethanolamine Pure is a colorless to yellow liquid with an amine-like odor. It is miscible with water in all proportions.Synonyms: Triethanolamine, 2,2',2'.. |
|||
| Density | 1.08 - 1.13 g/cc | 0.0390 - 0.0408 lb/in³ | |
| 3M Fastbond™ 100 Lavender Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
| Density | 1.08 - 1.13 g/cc | 0.0390 - 0.0408 lb/in³ | |
| 3M Fastbond™ 100 Neutral Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
| Density | 0.900 - 1.13 g/cc | 0.0325 - 0.0408 lb/in³ | Average value: 0.919 g/cc Grade Count:40 |
| Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
| Density | 1.11 - 1.13 g/cc | 0.0401 - 0.0408 lb/in³ | ASTM D792 |
| Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
| Density | 1.03 - 1.13 g/cc | 0.0372 - 0.0408 lb/in³ | Average value: 1.07 g/cc Grade Count:13 |
| Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |
|||