Physical Properties Metric English Comments
Density 13.8 - 14.1 g/cc
0.499 - 0.509 lb/in³
China Tungsten YG16C Cemented Tungsten Carbide for Mining Purposes
For oil cone drill bits for medium soft and medium hard rocks.Information provided by China Tungsten
Density 13.8 - 14.1 g/cc
0.499 - 0.509 lb/in³
China Tungsten ZY32 Tungsten Carbide for Mining Purposes
High toughness and wear resistance, for hi-speed wire mills for intermediate and finish rolling ,able to use for hard wires.Information provided by China Tungsten
Density 13.8 - 14.1 g/cc
0.499 - 0.509 lb/in³
China Tungsten ZY33 Tungsten Carbide for Mining Purposes
High toughness and wear resistance, for hi-speed wire mills for intermediate and finish rolling ,able to use for hard wires.Information provided by China Tungsten