Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.870 - 11.0 g/cc | 0.0314 - 0.397 lb/in³ | Average value: 1.06 g/cc Grade Count:952 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Density | 0.820 - 11.0 g/cc | 0.0296 - 0.397 lb/in³ | Average value: 1.42 g/cc Grade Count:484 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Density | 0.960 - 11.0 g/cc | 0.0347 - 0.397 lb/in³ | Average value: 1.26 g/cc Grade Count:92 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |