Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
Pacific Sintered Materials FN-262-T(HT) High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0408-155HTAll information provided by Pacific Sintered Metals. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals 4600 F-253-T(HT) Powdered Metal High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-140HTInformation Provided by Pacific Sintered Metals, a division of PSM .. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-256-T(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0408-155HTInformation Provided by Pacific Sintered Metals, a divis.. |
|||
Density | 7.20 - 7.40 g/cc | 0.260 - 0.267 lb/in³ | |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-T Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-45Information Provided by Pacific Sintered Metals, a division.. |
|||
Density | 6.80 - 7.40 g/cc | 0.246 - 0.267 lb/in³ | |
China Tungsten ST2270 PM Antifriction Parts Information provided by China Tungsten |