Polymer Property : Density = 0.170 lb/in³
Polymer Property :
Density =
0.170 lb/in³
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Density
4.10
-
4.70
g/cc
0.148
-
0.170
lb/in³
ASTM B212
H.C. Starck Amperit® 538.074 Agglomerated, Sintered Tungsten Carbide-Tungsten Boride-Cobalt (WC-WB-Co ) 60-30-10