Polymer Property : Density = 0.0802 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.18 - 2.22 g/cc
0.0788 - 0.0802 lb/in³
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne..
Density 1.95 - 2.22 g/cc
0.0704 - 0.0802 lb/in³
Apparent Density
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
Density 2.16 - 2.22 g/cc
0.0780 - 0.0802 lb/in³
ASTM D792
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..
Density 1.95 - 2.22 g/cc
0.0704 - 0.0802 lb/in³
Momentive Performance Materials Pyrolytic Boron Nitride (PBN) Coating
High temperature protective coating for graphite.PBN has become the material of choice for compound semiconductor crystal growth and wafer processing. PBN coatings also seal and protect graphite fr..
Density 2.19 - 2.22 g/cc
0.0791 - 0.0802 lb/in³
molded; ASTM D792
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..