Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.73 - 1.88 g/cc | 0.0626 - 0.0678 lb/in³ | |
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |