Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.11 - 1.57 g/cc | 0.0401 - 0.0567 lb/in³ | Average value: 1.43 g/cc Grade Count:98 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Density | 1.27 - 1.57 g/cc | 0.0459 - 0.0567 lb/in³ | Average value: 1.40 g/cc Grade Count:31 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.20 - 1.57 g/cc | 0.0434 - 0.0567 lb/in³ | Average value: 1.29 g/cc Grade Count:32 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 324 Rigid PVC, Extrusion Furniture profiles |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 418 Rigid PVC, Extrusion Electric channels |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion Antishock pipes and profiles |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 330 Rigid PVC, Extrusion Lead Free Profiles |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 78 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 80/1 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 83 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 89 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/15 Halogen Free PVC General purpose |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 019/G Halogen Free PVC Sheathing; high flexibility |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4523 Halogen Free PVC High flame retardancy |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds R 220 Rigid PVC, Extrusion Rolling shutters |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds R 220/R Rigid PVC, Extrusion Shiny rolling shutters |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 86 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 89 Flexible PVC, Flame Retardant Insulation Power cables |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 225/R Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Density | 1.36 - 1.57 g/cc | 0.0491 - 0.0567 lb/in³ | Average value: 1.45 g/cc Grade Count:30 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Density | 1.54 - 1.57 g/cc | 0.0556 - 0.0567 lb/in³ | Average value: 1.56 g/cc Grade Count:5 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |