Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
Novatec Novacycle® 501 PVC Novacycle® 501 is a general purpose, rigid, extrusion grade PVC compound in pellet form. This formulation is designed to provide an economical alternative for extruded profiles Raw material appe.. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or .. |
|||
Density | 1.20 - 1.37 g/cc | 0.0434 - 0.0495 lb/in³ | Average value: 1.26 g/cc Grade Count:19 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Density | 1.14 - 1.37 g/cc | 0.0412 - 0.0495 lb/in³ | Average value: 1.17 g/cc Grade Count:14 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Density | 1.12 - 1.37 g/cc | 0.0405 - 0.0495 lb/in³ | Average value: 1.19 g/cc Grade Count:15 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds RKS 300 Rigid PVC, Antishock Extrusion Lead Free Dielectric conduits, antishock |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds RST 171 Rigid PVC, Extrusion Lead Free Various transparent profiles |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
KYDEX® 6185 Thermoplastic Sheet High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar.. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® LB C076 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | Fiber Density |
SGL Carbon Group PANOX® LB S004 EEA Oxidized Textile Fiber, Staple Fiber, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Density | 1.31 - 1.37 g/cc | 0.0473 - 0.0495 lb/in³ | |
Dow BETAMATE™ XW 1044-3 Epoxy BETAMATE™ XW 1044-3 is a one component, epoxy based adhesive especially developed for the body shop. The adhesive can be applied by robot systems and it shows high adhesion to metal and non-metal .. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 80/R Flexible PVC, Sheathing General purposes (90°) |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds FK 70 Flexible PVC, Insulation Lead Free General purposes |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7430 Flexible PVC, Injection Molding for Footwear Sandals |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 100/2 Flexible PVC, Insulation for High Temperatures Operating temperature 80°C |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 120 Flexible PVC, Insulation for High Temperatures Operating temperature 110°C |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds ART 10 Rigid PVC, Atoxic for General Purpose Transparent bottles medium antishock |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds CL 7830 Flexible PVC, Sheathing Sheath coaxial TV Cable |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds GSK 6635 Flexible PVC, Injection Molding, Lead Free Items for contact ABS |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 120/1 Flexible PVC, Insulation for High Temperatures Operating temperature 110°C |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds HL 96/2 Flexible PVC, Insulation for High Temperatures Low thickness cable for car |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1184 |
Fainplast Compounds KL 84/1 Flexible PVC, Insulation for High Temperatures Lead Free General purposes flame retardant |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 100 Flexible PVC, Lead Free Semi-rigid extrusion for handrail |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 7540/N Flexible PVC, Lead Free Profiles according to norm EN 71/3 |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 9220 Flexible PVC, Lead Free Fencing |
|||
Density | 1.32 - 1.37 g/cc | 0.0477 - 0.0495 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Injection Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft flow Applications:Telecommunication .. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 67/FR Flexible PVC, Lead Free Spiral pipes, UL 94 Class V0 |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet
(discontinued **) Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical.. |
|||
Density | 1.33 - 1.37 g/cc | 0.0480 - 0.0495 lb/in³ | ASTM D792 |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |