Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.895 - 0.915 g/cc | 0.0323 - 0.0331 lb/in³ | Average value: 0.904 g/cc Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |