Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.815 - 0.862 g/cc | 0.0294 - 0.0311 lb/in³ | |
Lord Adhesives Chemlok® 5151 Adhesive Chemlok® 5151 is a single coat adhesive used to bond fluorocarbon based elastomers to metal. It is particularly effective on phosphate coated metals. Chemlok 5151 adhesive will bond a wide variet.. |