Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.480 - 0.640 g/cc | 0.0173 - 0.0231 lb/in³ | |
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |
|||
Density | 0.481 - 0.641 g/cc | 0.0174 - 0.0231 lb/in³ | Dry |
Unifrax Fiberfrax® Vari-Form™ A Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Density | 0.577 - 0.641 g/cc | 0.0208 - 0.0231 lb/in³ | |
Engineered Syntactic Systems AZ-38 Deep Water Syntactic Foam Syntactic foams are a combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high c.. |
|||
Density | 0.577 - 0.641 g/cc | 0.0208 - 0.0231 lb/in³ | |
Engineered Syntactic Systems SF-38 Subsea Syntactic Void Filler SF-38 is a specially engineered syntactic formulated to serve as a void filler for subsea applications. The material is provided as a three-part kit that is mixed and poured into any free-flood cavi.. |
|||
Density | 0.577 - 0.641 g/cc | 0.0208 - 0.0231 lb/in³ | |
Engineered Syntactic Systems MZ-38 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |