Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.150 - 0.190 g/cc | 0.00542 - 0.00686 lb/in³ | ISO 845-88 |
Eurofoam Porocell 251 BG NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |