Polymer Property : Density = 0.00506 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.110 - 0.140 g/cc
0.00397 - 0.00506 lb/in³
ASTM D792
Microcell Composite Company CELLIFF® F7010 Polymer Foam
CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr..
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ASTM D792
Microcell Composite Company CELLOMER® S-2110 SBS Rubber Foam
CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by..
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ASTM D792
Microcell Composite Company CELLOMER® S-2110D SBS Rubber Foam
CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by..
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ASTM D792
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam
CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high..
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 301/F NR-SBR Foam
Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-RS EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.120 - 0.140 g/cc
0.00434 - 0.00506 lb/in³
ISO 845-88
Eurofoam Siliconcell 414/0 Silicone Foam
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-BI EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
3M K1 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-GR EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ASTM D792
Microcell Composite Company CELLAMP® M5110 Thermoplastic Foam
CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high d..