Polymer Property : Density = 0.00415 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0850 - 0.115 g/cc
0.00307 - 0.00415 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 B-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.0900 - 0.115 g/cc
0.00325 - 0.00415 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Density 0.105 - 0.115 g/cc
0.00379 - 0.00415 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu..