Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.00800 - 0.0120 g/cc | 0.000289 - 0.000434 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova T243C Expandable Polystyrene A fast expanding regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent typically used for low and standard density foam.Applications: This grade is us.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect G Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect G+ Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect UF Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect V3012 Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect UL Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect W Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |
|||
Density | 0.00400 - 0.0120 g/cc @Pressure 0.1013 MPa, Temperature 20.0 °C |
0.000145 - 0.000434 lb/in³ @Pressure 14.69 psi, Temperature 68.0 °F |
|
BASF Basotect TG Foam Basotect® is a flexible, open cell foam made from melamine resin, a thermoset polymer. Its characteristic feature is its three-dimensional network structure consisting of slender and thus easily sh.. |