Polymer Property : Density = 0.679 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 18.8 g/cc
0.679 lb/in³
Wieland BioPorta G PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental
Density 18.8 g/cc
0.679 lb/in³
Wieland Porta REFLEX® PFM Alloy
Gold-platinum ceramic alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneering, acrylic veneeringDental