Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 14.2 g/cc | 0.513 lb/in³ | |
Wieland Porta Aurium 2 PFM Alloy All-purpose alloy for low-fusing high expanding ceramicsApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, ceramic veneerin.. |
|||
Density | 14.2 g/cc | 0.513 lb/in³ | |
China Tungsten YG13C Tungsten Carbide Powder Information provided by China Tungsten |
|||
Density | 14.2 g/cc | 0.513 lb/in³ | |
China Tungsten YG13X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Density | 14.2 g/cc | 0.513 lb/in³ | |
China Tungsten YT726 Tungsten Carbide High red hardness and wear resistance. Turning and Milling of chilled cast irons, cast alloy irons and quenched steelInformation provided by China Tungsten |